AWS: SFA 5.4 E318-16 Stainless Steel Welding Electrodes, Best Welding Rods

Inkcazelo emfutshane:

I-A212 (i-AWS E318-16) i-electrode yensimbi engenasici ephantsi kwe-carbon Cr18Ni12MoNb ene-niobium-containing stabilizer ene-titanium-calcium coating.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Stainless Steel Welding Electrode

A212

GB/T E318-16

AWS A5.4 E318-16

Inkcazo: I-A212 yi-carbon ephantsi ye-Cr18Ni12MoNb ye-electrode yensimbi engenasici kunye ne-niobium-containing stabilizer ene-titanium-calcium coating.Ingasetyenziselwa zombini i-AC kunye ne-DC ngokusebenza okugqwesileyo kokusebenza.Intsimbi ediphozithiweyo inomsebenzi ongcono we-intergranular corrosion kune-A202 kunye ne-A207.

Isicelo: Isetyenziselwa i-welding ebalulekileyo ye-06Cr17Ni12Mo2, i-ultra-low carbon Cr17Ni14Mo2 kunye nezinye izakhiwo zensimbi ezingenasici, ezifana ne-urea synthesis tower, izixhobo ze-vinylon kunye nezinye iindawo ezivezwe kwimithombo yeendaba ezomeleleyo.

 

 

Ukwakhiwa kweekhemikhali zentsimbi edibeneyo(%):

C

Mn

Si

Cr

Ni

Nb

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

17.0 ~ 20.0

11.0 ~ 14.0

6 XC ~ 1.00

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Iimpawu zobuchwephesha bentsimbi ye-weld:

Into yovavanyo

Tensile strength

Mpa

Elongation

%

Iqinisekisiwe

≥550

≥25

 

yangoku eCetyisiweyo:

Intonga yobubanzi

(mm)

2.0

2.5

3.2

4.0

5.0

I-Welding yangoku

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Isaziso:

1. I-electrode kufuneka ibhakwe ngeyure eli-1 malunga ne-150 ℃ ngaphambi kokusebenza kwe-welding;

2. Ngenxa yokuba ubunzulu bokungena bunzulu ngexesha lokuwelda kwe-AC, unikezelo lombane lwe-DC kufuneka lusetyenziswe kangangoko ukufumana ukungena nzulu.kwaye umsinga akufanele ube mkhulu kakhulu ukuphepha ubomvu bentonga ye-welding;

3. Ukuxhatshazwa kwe-corrosion yensimbi egciniweyo kunqunywe yisivumelwano esiphindwe kabini sokubonelela kunye nemfuno.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Siye sazixakekisa ekwenzeni ii-electrode zokuwelda, iintonga ze-welding, kunye nezinto ezisetyenziselwa ukuwelda iminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka i-electrode yentsimbi ye-welding, i-carbon steel welding electrode, i-alloy welding electrode, i-electrode ye-welding, i-nickel & ne-cobalt alloy welding electrode, intsimbi ethambileyo kunye ne-low alloy welding wires, i-welding steel wire, i-gas-shielded flux cored wire, iingcingo ze-aluminiyam, ukuwelda kwe-arc emanzini.iingcingo, i-nickel & ne-cobalt alloy welding ingcingo, iingcingo zokuwelda zobhedu, i-TIG & ne-MIG iingcingo zokuwelda, ii-electrode ze-tungsten, i-carbon gouging electrode, kunye nezinye izincedisi ze-welding & consumables.

 

 