I-D256 (B-80) i-Hardfacing Welding Electrode, i-Welding Rod, i-Welding Stick.

Inkcazelo emfutshane:

I-electrode esisiseko edipozitha intsimbi ye-austenitic manganese, ethi iqina ngoguquko olubandayo, esebenza kwiintsimbi zokwakheka okufanayo nakwiindawo eziphantsi kweempembelelo ezimandundu kunye nokugruzuka okuphakathi.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Hardfacing Welding Stick ElectrodeURODO P

RODO PARA RECUBRIMIENTO UMKHUSELI

Uhlobo lweNombolo: D256 (B – 80)

Uhlalutyo lweMetal eDiphozithiweyo (Amaxabiso aqhelekileyo)

C

1.2%

Mn

13.0%

Si

0.5%

Ni

3.0%

 

Iimpawu:

I-electrode esisiseko edipozitha intsimbi ye-austenitic manganese, ethi iqina ngoguquko olubandayo, esebenza kwiintsimbi zokwakheka okufanayo nakwiindawo eziphantsi kweempembelelo ezimandundu kunye nokugruzuka okuphakathi.Kukulungele ukubuyiswa, ukugquma kunye nokulungiswa kweentsimbi ze-austenitic Mn, iinxalenye kunye neziqwenga zoomatshini abanzima.

 

Iinkcazelo ngoomatshini:Ubunzima 200-250 HB BRINELL kwidiphozithi, 300-400 HB Brinell

emva komsebenzi obandayo wokuqina.

 

Izikhundla zeWelding:Umcaba, othe tye, oPhezulu, othe nkqo phezulu.

 

Ngoku kunye nePolarity:

Ngokutshintshana okanye ngqo ngoku

i-electrode ukuya kwipali efanelekileyo

ewe mm

o kwi

Amperage

3.20

1/8

110-130

4.00

5/32

140-160

5.00

2/16

180-230

 

Usetyenziso: • Ukuzalisa iintsimbi zeManganese.

• Ukwakhiwa ngokutsha kwamazinyo e-excavator kunye nee-emele.

• Ukunqumla kunye neentliziyo zeereyili.

• Izingqusho zeminerali kunye neehamile.

• Ngokubethelela ubunzima bayo bunyuka ukuya kuma-350 – 400 HB.

• Xa usakha ngokutsha okanye uhombisa, sebenzisa i-AG AR-91 njengesiseko.

• Kubushushu obungaphezulu kwe-300 OC, iintsimbi ze-Mn

Baqala ukulahlekelwa ubunzima.Iileyisi ziyacetyiswa

ukutsiba, ubuncinane bedayamitha kunye ne-amperage enokwenzeka.

 

 

UBUDE: 350mm.

Ubunzima NGEBHOKISI NGANYE: 20 kg/44 lbs.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Siye sabandakanyeka ekwenzenii-electrode ye-weldings, iintonga ze-welding, kunye ne-welding consumables iminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka insimbi engenasicii-electrode ye-weldings, carbon steel welding electrode, low alloy welding electrode, surfacing welding electrode, nickel & cobalt alloy welding electrode, mild steel & low alloy welding wires, steel stainless steel welding wires, flux cored cored wires, aluminiyam welding wires, submerged arc welding .iingcingo, i-nickel & ne-cobalt alloy welding ingcingo, iingcingo zokuwelda zobhedu, i-TIG & ne-MIG iingcingo zokuwelda, ii-electrode ze-tungsten, i-carbon gouging electrode, kunye nezinye izincedisi ze-welding & consumables.

 

 

 

 


  • Ngaphambili:
  • Okulandelayo: