I-B-85 i-Hardfacing Welding Electrode, i-Surfacing Welding Rod, i-Arc Welding Stick

Inkcazelo emfutshane:

I-coating yale electrode inomxholo ophezulu we-chromium, okwenza idiphozithi yayo ixhathise kakhulu ukunxitywa ngenxa yokukrala okugqithisileyo, ukukhuhlana okukhulu kunye neempembelelo eziphantsi, nakwiqondo lokushisa eliphezulu kunye ne-atmospheres ephazamisayo.Akufunekanga ibe sesichengeni kukothuka kakhulu okanye impembelelo.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Hardfacing Welding Stick Electrode

RECUBRIMIENTO UMKHUSELI

Uhlobo lweNombolo:B – 85

Uhlalutyo lweMetal eDiphozithiweyo (Amaxabiso aqhelekileyo)

C

4.0%

Si

0.6%

Cr

35%

 

Iimpawu:

I-coating yale electrode inomxholo ophezulu we-chromium, okwenza idiphozithi yayo ixhathise kakhulu ukunxitywa ngenxa yokukrala okugqithisileyo, ukukhuhlana okukhulu kunye neempembelelo eziphantsi, nakwiqondo lokushisa eliphezulu kunye ne-atmospheres ephazamisayo.Akufunekanga ibe sesichengeni kukothuka kakhulu okanye impembelelo.

 

Iinkcazelo ngoomatshini:Ubunzima ukusuka kwi-57 ukuya kwi-62 Hrc.(Amaqweqwe amabini)

 

Ngoku kunye nePolarity:

Ukutshintsha okukhethiweyo okwangoku ngoku ngokuthe ngqo, i-electrode ukuya kwipali elungileyo

ewe mm.

1/8”

5/32”

3/16”

Amp.min.

120

170

220

Amp.max.

140

190

250

 

Usetyenziso:

• Icoat screw conveyors

• Amabhakethi e-excavator

• Amazinyo e-scarifier

• Iimpompo zokukhupha amanzi

• Oomatshini bemigodi

• Iimpompo zesanti

 

 

UBUDE: 350mm.

Ubunzima NGEBHOKISI NGANYE: 20 kg/44 lbs.

 

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Siye sabandakanyeka ekwenzenii-electrode ye-weldings, iintonga ze-welding, kunye ne-welding consumables iminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka i-electrode yentsimbi ye-welding, i-carbon steel welding electrode, i-alloy welding electrode, i-electrode ye-welding, i-nickel & ne-cobalt alloy welding electrode, intsimbi ethambileyo kunye ne-low alloy welding wires, i-welding steel wire, i-gas-shielded flux cored wire, iingcingo ze-aluminiyam, ukuwelda kwe-arc emanzini.iingcingo, i-nickel & ne-cobalt alloy welding ingcingo, iingcingo zokuwelda zobhedu, i-TIG & ne-MIG iingcingo zokuwelda, ii-electrode ze-tungsten, i-carbon gouging electrode, kunye nezinye izincedisi ze-welding & consumables.

 

 

 

 


  • Ngaphambili:
  • Okulandelayo: