I-AWS A5.1 E7028 Intonga yokuWeldas
I-Welding electorde AWS A5.1 E7028 yi-electrode yentsimbi yekhabhoni egqunywe yi-hydrogen-potassium-iron-powder ephantsi. Umgubo wesinyithi okwi-coating unyusa izinga lokufakwa kwe-deposit ukuya kuthi ga kwi-180%. Inokusebenziseka kakuhle kakhulu okwenza ukuba ibe ne-arc ezinzileyo, i-spatter ephantsi, ukususwa kwe-slag kulula kwaye yenza i-welding ye-all-position. Isinyithi esigciniweyo sineempawu ezilungileyo zoomatshini ezibonelela ngokuqina okuhle kakhulu kubushushu obuphantsi.
Isicelo
I-AWS A5.1 E7028 isetyenziswa kwi-flat and flat fillet welding kwizakhiwo ezenziwe nge-carbon steel kunye ne-low alloy steels ezifana ne-16Mn, 09Mn2Si kunye ne-A, B, D, E steels ezisetyenziswa ekwakheni iinqanawa.
Ulwakhiwo lweeKhemikhali (%)
| Ukwenziwa kweeKhemikhali | C | Mn | Si | S | P | Ni | Cr | Mo | V |
| Ixabiso leSiqinisekiso | ≤0.15 | ≤1.60 | ≤0.90 | ≤0.035 | ≤0.035 | ≤0.30 | ≤0.20 | ≤0.30 | ≤0.08 |
| Isiphumo Jikelele | 0.077 | 1.03 | 0.35 | 0.005 | 0.014 | 0.011 | 0.028 | 0.007 | 0.016
|
Iipropati zoomatshini zesinyithi esigciniweyo
| Into yoVavanyo | I-Rm (N/mm2) | I-Rel (N/mm2) | I-A (%) | KV2(J) -30°C |
| Ixabiso leSiqinisekiso | ≥490 | ≥400 | ≥20 | ≥27 |
| Isiphumo Jikelele | 535 | 430 | 26 | 189 |
Isalathiso sangoku (DC)
| Ububanzi | φ4.0 | φ5.0 |
| I-Amperage | 180 ~ 240 | 210 ~ 280 |
Amanqaku:
1. I-electrode mayifudunyezwe kubushushu obuyi-350°C kangangeyure e-1. Fudumeza intonga nanini na xa isetyenziswa.
2. Ukungcola okufana nomhlwa, amabala eoyile kunye nokufuma kufuneka kususwe kwindawo yokusebenza.
3. Kufuneka i-arc emfutshane ukuze kwenziwe i-welding. Indlela encinci yokuwelda iyathandwa.
Ukugcinwa kunye nokubhaka kwe-E7028 Welding Electrode
Ekubeni i-electrode ye-hydrogen ephantsi, i-E7016 ifunaukubhaka/ ukomisangaphambi kokusetyenziswa. Ubushushu obucetyiswayo bokomisa okanye bokubhaka kwi-E7028 rod ngokwe-AWS A5.1, Itheyibhile 1.3 yi-500-800°F (260-425°C) kangangeyure e-1-2.
I-electrode ebhakiweyo okanye eyomileyo mayigcinwe kwi-oven ephathwayo kubushushu obuyi-50-250°F (30-140°C) ngexesha lokusetyenziswa. I-electrode engasetyenziswanga mayibuyiselwe kwii-oven ezihlala zihleli.