I-ER70S2 yintambo ye-MIG kunye ne-TiG ekumgangatho ophezulu yokuwelda kuzo zonke iintlobo zeentsimbi ezithambileyo nezekhabhoni, ivelisa ii-welds ezisemgangathweni ezine-porosity encinci. Yintambo ye-triple deoxidized (i-Zirconium, i-Titanium, kunye ne-Aluminium) eyenza ukuba ibe lukhetho oluhle kakhulu lokuwelda phezu komhlwa kunye nesikali se-mill. Akukho flux ifunekayo kule mveliso.
ISICELO ESIQHELEKILEYO:
imibhobho kunye nezixhobo zokugrumba ezikude nolwandle, umsebenzi wesinyithi wolwakhiwo
| Indawo yokuWelda: F, V, OH, H | Okwangoku: DCEP |
| Amandla okuThamba, kpsi: | 70 |
| Amandla okuvelisa, kpsi: | 58 |
| Ukwandiswa kwi-2”%: | 22 |
I-Charpy V-Notch eqhelekileyo: 35 ft.-lb. Kwi -20 deg F
I-Cystemi yeNtambo eqhelekileyo ngokwe-AWS A5.18 (amaxabiso alinganayo aphezulu)
| C | Mn | Si | P | S | Ni | Cr | Mo | V | Cu | Ti | Zr | Al | ||
| 0.07 | 0.90-1.40 | 0.40-0.70 | 0.025 | 0.035 | 0.15 | 0.15 | 0.15 | 0.03 | 0.50 | 0.05-0.15 | 0.02-0.12 | 0.05-0.15 | ||
| Iiparameters zeWelding eziqhelekileyo | ||||||||||||||
| Ububanzi | Inkqubo | I-Volt | Ii-Amps | Igesi yokukhusela | ||||||||||
| in | (mm) | |||||||||||||
| .035 | (0.9) | I-GMAW | 28-32 | 165-200 | Ukudluliselwa kweSpray 98% Argon+2% Oxygen okanye 75% Argon+25% CO2 | |||||||||
| .045 | (1.2) | I-GMAW | 30-34 | 180-220 | Ukudluliselwa kweSpray 98% Argon+2% Oxygen okanye 75% Argon+25% CO2 | |||||||||
| 1/16 | (1.6) | I-GMAW | 30-34 | 230-260 | Ukudluliselwa kweSpray 98% Argon+2% Oxygen okanye 75% Argon+25% CO2 | |||||||||
| .035 | (0.9) | I-GMAW | 22-25 | 100-140 | Ukudluliselwa kwe-100% CO2 okanye i-75% Argon +25% CO2 | |||||||||
| .045 | (1.14) | I-GMAW | 23-26 | 120-150 | Ukudluliselwa kweSekethe emfutshane yi-100% CO2 okanye i-75% Argon +25% CO | |||||||||
| 1/16 | (1.6) | I-GMAW | 23-26 | 160-200 | Ukudluliselwa kweSekethe emfutshane yi-100% CO2 okanye i-75% Argon +25% CO | |||||||||
| .035 | (0.9) | I-GTAW | 13-16 | 60-100 | I-Argon eyi-100% | |||||||||
| .045 | (1.14) | I-GTAW | 13-16 | 70-120 | I-Argon eyi-100% | |||||||||
| 1/16 | (1.6) | I-GTAW | 12-15 | 100-125 | I-Argon eyi-100% | |||||||||
| 3/32 | (2.4) | I-GTAW | 15-20 | 125-175 | I-Argon eyi-100% | |||||||||
| 1/8 | (3.2) | I-GTAW | 15-20 | 175-250 | I-Argon eyi-100% | |||||||||