Iintambo zokuWelda zentsimbi yekhabhoni ze-ER70S-3, iintsimbi zokuzalisa zentambo yokuWelda ye-Arc ekhuselweyo yegesi, i-Tig kunye ne-Mig Wire

Inkcazo emfutshane:

I-ER70S3 yintambo ye-MIG esetyenziswa ngokubanzi efanelekileyo kwiintlobo ezininzi ze-carbon steel welding.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-ER70S-3 CARBON STEEL Filler Metals yoShicilelo lwe-Arc oluKhuselekileyo lweGesi

I-ER70S3 yintambo ye-MIG esetyenziswa ngokubanzi efanelekileyo kwiintlobo ezininzi ze-carbon steel welding. Yintambo ye-silicon kunye ne-manganese deoxidized eyenza ukuba ibe ntle kakhulu kwimveliso eqhelekileyo. Le mveliso ifuna igesi yokukhusela.

Izicelo eziqhelekileyo: ukwenziwa ngokubanzi, ifenitshala yesinyithi, ishiti yesinyithi, ukwenziwa kwesinyithi sokuhombisa, izixhobo zasefama

Iklasi ye-AWS: ER70S3 Isiqinisekiso: AWS A5.18/A5.18M:2005
I-alloy: ER70S3 I-ASME SFA A5.18

 

Indawo yokuWelda: F, V, OH, H Okwangoku:
I-MIG-DCEP
I-TIG-DCEN

 

Amandla okuThamba, kpsi: 70
Amandla okuvelisa, kpsi: 58
Ukwandiswa kwi-2”%: 22

I-Cystemi yeNtambo eqhelekileyo ngokwe-AWS A5.18 (amaxabiso alinganayo aphezulu)

C Mn Si P S Ni Cr Mo V Cu
0.06-0.15 0.90-1.40 0.45-0.75 0.025 0.035 0.15 0.15 0.15 0.03 0.50
Iiparameters zeWelding eziqhelekileyo
Ububanzi Inkqubo I-Volt Ii-Amps Igesi yokukhusela
in (mm)
.035 (0.9) I-GMAW 28-32 165-200 Ukudluliselwa kweSpray 98% Argon+2% Oxygen okanye 75% Argon+25% CO2
.045 (1.2) I-GMAW 30-34 180-220 Ukudluliselwa kweSpray 98% Argon+2% Oxygen okanye 75% Argon+25% CO2
1/16 (1.6) I-GMAW 30-34 230-260 Ukudluliselwa kweSpray 98% Argon+2% Oxygen okanye 75% Argon+25% CO2
.035 (0.9) I-GMAW 22-25 100-140 Ukudluliselwa kwe-100% CO2 okanye i-75% Argon +25% CO2
.045 (1.2) I-GMAW 23-26 120-150 Ukudluliselwa kweSekethe emfutshane yi-100% CO2 okanye i-75% Argon +25% CO
1/16 (1.6) I-GMAW 23-26 160-200 Ukudluliselwa kweSekethe emfutshane yi-100% CO2 okanye i-75% Argon +25% CO
1/16 (1.6) I-GTAW 12-15 100-125 I-Argon eyi-100%
3/32 (2.4) I-GTAW 15-20 125-175 I-Argon eyi-100%
1/8 (3.2) I-GTAW 15-20 175-250 I-Argon eyi-100%

 