I-electrode yokuwelda ye-E410NiMo-15

Inkcazo emfutshane:

I-E410NiMo-15 yi-electrode yokuwelda yentsimbi engagqwali ye-martensitic ene-hydrogen sodium-coating ephantsi eyi-11.0-12.5% ​​Cr, 4.0-5.0 Ni, kunye ne-0.40-0.70% Mo.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Umgangatho ohambelanayo

GB/T 983-2012 E410NiMo-15

I-AWS A5.4M-2012 E410NiMo-15

Izinto ezilinganayo:1.4317 GX4CrNi13-4,1.4313 X3CrNiMo13-4,1.4407 GX5CrNiMo13-4,1.4414 GX4CrNiMo13-4,ACI Gr. I-CA6NM,UNS S41500

Inkcazo

I-E410NiMo-15 yi-electrode yokuwelda yentsimbi engagqwali ye-martensitic ene-hydrogen sodium coating ephantsi, equlethe i-11.0-12.5% ​​Cr, 4.0-5.0% Ni, kunye ne-0.40-0.70% Mo. Ifanelekile kwi-arc welding yentsimbi ekhuselweyo (i-SMAW) ene-arc ezinzileyo, i-spatter encinci, kunye nokuqhekeka kwe-slag okugqwesileyo. Isinyithi esigciniweyo sinika amandla aphezulu, ukumelana nokugqwala okuhle, kunye nokumelana nokuqhekeka. Kucetyiswa ukufudumeza kwiindawo zokusebenza ezixineneyo, kwaye unyango lobushushu emva kokuwelda (i-PWHT) luyimfuneko kwi-580~620℃ (iiyure ezi-1-2, ukupholisa umoya, i-AC).

Isicelo

Ilungele ukuwelda intsimbi eqhotsiweyo ye-ASTM CA6NM, iintsimbi zochungechunge lwe-13%Cr-4%Ni (umz., i-Cr13Ni4Mo, i-Cr13Ni5Mo), kunye neentsimbi ezifanayo ze-martensitic stainless. Izicelo eziqhelekileyo ziquka ukuwelda ukulungisa ii-hydropower turbine runners, imizimba yeevalvu, iipayipi zoxinzelelo oluphezulu, kunye nomphezulu wezinto ezigutyungelwe yi-cavitation. Ikwasetyenziselwa ukulungisa iindawo eziqinileyo ezinganyangekiyo njengee-crusher rolls kunye nee-pump casings.

Ukwakheka kweekhemikhali zeWeld Metal (%)

I-elementi C Mn Si P S Cr Ni Mo Cu
Imfuneko ≤0.06 ≤1.0 ≤0.90 ≤0.04 ≤0.03 11.0-12.5 4.0-5.0 0.40-0.70 ≤0.75
Iziphumo zovavanyo 0.029 0.7 0.32 0.028 0.01 12.26 4.50 0.55 0.01

Iipropati zoomatshini zesinyithi esigciniweyo

Igama lovavanyo Amandla okuThamba (i-Mpa) Ukwandiswa% I-X-Rey Uvavanyo lweMpembelelo, (+20℃)J Ubunzima be-HB I-Hydrogen enyibilikayo (ml/100g)
Imfuneko ≥760 ≥15 Ibanga loku-1 – – ≤5
Iziphumo zovavanyo 845 19 Ibanga loku-1 60-90 250-310 ≤5

Iiparameters zokuWelding ezicetyiswayo

Umthombo wamandla: DC Reserve (DC-)

I-Current ecetyiswayo

Ububanzi bentonga (mm) 3.2 4.0 5.0
Ukuwelda Ngoku (A) 80-120 120-160 150-190

Isaziso:

1. Bhaka i-electrode kwi-300℃ kangangeyure ngaphambi kokuba uyisebenzise ukususa umswakama.
2.Coca umhlwa, ioyile, kunye nokufuma kumphezulu wesinyithi osisiseko; sebenzisa umsebenzi omfutshane we-arc kwiintsimbi ezimxinwa ze-weld.
3. I-PWHT kufuneka yenziwe ngoko nangoko emva kokuwelda ukuze kuthintelwe ukuqhekeka.

  • Ngaphambili:
  • Okulandelayo: