H10MnSi AWS EM13K Submerged Arc Welding Wire

Inkcazelo emfutshane:

I-H10MnSi I-arc welding wire efakwe emanzini luhlobo lwe-medium-manganese kunye ne-medium-silicon type welding wire.


Iinkcukacha zeMveliso

Iithegi zeMveliso

H10MnSi AWS EM13K Submerged Arc Welding Wire

EM13K 2.5/3.2/4.0/5.0mm Submerged Arc Welding Wire

I-H10MnSi I-arc welding wire efakwe emanzini luhlobo lwe-medium-manganese kunye ne-medium-silicon type welding wire.
1. Ihambelana ne-medium-manganese kunye ne-medium-silicon type welding flux.
2. Ayinabungozi kwi-rust kwisiseko sesinyithi.
3. Inobunjwa obugqwesileyo be-bead kunye ne-slag dechability.
4. I-Monopole okanye i-dipole.U-AC DC.
5. Isetyenziselwa zombini isantya esiphezulu se-welding kunye nokuzalisa i-welding kwi-50kg yesiseko sesinyithi seklasi.
6. i-welding yenye i-501 Mpa level carbon steel kunye nentsimbi ephantsi ye-alloy

I-EM13K ihambelana noMgangatho :GB/T 5293 H10MnSi
AWS EM13K
ISO 14171-B-SU25

Ukucaciswa:Luhlobo locingo lwe-welding olunomxholo ofanelekileyo wemanganese kunye nesilicon.,Ihambelana ne-manganese ephantsi kunye ne-silicon ephantsi yohlobo lwe-welding flux,Ayikhathaleli kumhlwa kwisiseko sesinyithi.Inobunjwa obugqwesileyo be-bead, isakhono esigqwesileyo se-slag.

Injongo: Ukusetyenziswa nge-sintered flux L.SJ101, ingasetyenziselwa zombini kwi-high-speed welding steel plate yamandla e-tensile 420N / mm2 kunye nokuzalisa i-welding.Isetyenziswa ngokubanzi kwibhoyila yokuwelda, inqanawa yoxinzelelo, ibhulorho, inqanawa njl.

Ukwakhiwa kwemichiza(%)

 

 

Ukuqulunqwa kwemichiza C Mn Si S P Cr Ni Cu
Ixabiso lesiqinisekiso ≤0.14 0.80~
1.10
0.60~
0.90
≤0.035 ≤0.035 ≤0.20 ≤0.30 ≤0.35
Isiphumo ngokubanzi 0.089 0.98 0.67 0.023 0.032 0.015 0.034 0.11

 
IiPropati zeMechanical zeMetal eDiphozithiweyo

Into yovavanyo

Flux

Rm(MPa) ReL/Rp0.2(MPa) A(%) I-KV2(J)
-20℃
I-LT•SJ101 415~550 ≥330 ≥22 ≥27

 
Ubungakanani beeNcingo zeWelding

Ubungakanani(mm) Φ2.5 Φ3.2 Φ4.0 Φ5.0

 


  • Ngaphambili:
  • Okulandelayo: