Ii-Electrode ze-Welding eziqinileyo ze-DIN 8555 (E1-UM-350) ii-Welding Rods eziMphezulu, Nxiba i-Electrode ye-Resistant Stick

Inkcazelo emfutshane:

I-DIN 8555 (E1-UM-350) yi-electrode ye-SMAW egqunyiweyo yokuqhekeka kunye nokunxiba i-surfacing enganyangekiyo.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Hardfacing WeldingI-Electrode

 

Umgangatho: DIN 8555 (E1-UM-350)

Uhlobo lweNombolo: TY-C DUR 350

 

Inkcazo kunye nesicelo:

· I-electrode ye-SMAW eqatyiweyo esisiseko yokuqhekeka kunye nokunxiba i-surface resistant.

· Ukumelana kakuhle nokukrazuka.Kulula ukuwelda kuzo zonke izikhundla.

· Ifaneleke ngokukodwa ukunxitywa kwe-surfacing ekwaziyo ukumelana ne-Mn-Cr-V alloyed parts, njengamasele, ii-track rollers, i-chain support rolls, i-sprocket wheels, i-guide rolls njl.njl.

 

Ukwakheka kweekhemikhali zentsimbi egciniweyo(%):

 

C

Si

Mn

Cr

Fe

I-DIN

-

-

-

-

-

EN

-

-

-

-

-

Isiqhelo

0.20

1.2

1.40

1.8

UBhal.

 

 

Ukuqina kwentsimbi efakiweyo:

Njengoko Welded

(HB)

Umaleko omnye kwintsimbi ene-C=0.5%

(HB)

370

420

 

Iimpawu eziqhelekileyo:

· Microstructure Ferrite + Martensitic

· Machinability Good nge Tungsten carbides tips izixhobo

· Ukufudumeza kwangaphambili Ukufudumeza iindawo ezinzima kunye neentsimbi ezinokuqina okuphezulu ukuya kwi-250-350 ℃

· Ukwenza i-Redry ye-2 h kwi-300℃ phambi kokusetyenziswa.

 


  • Ngaphambili:
  • Okulandelayo: