Inkcazelo emfutshane:

I-A107 (AWS E308-15) yi-carbon ephantsi ye-Cr19Ni10 i-electrode yensimbi engenasici kunye ne-low-hydrogen sodium coating.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Stainless Steel WeldingI-Electrode

A107                                        

GB/T E308-15

AWS E308-15

Inkcazo: I-A107 yi-electrode yentsimbi ephantsi ye-Cr19Ni10 ene-low-hydrogen sodium.Sebenzisa i-DCEP (i-electrode echanekileyo yangoku) kwaye inokudityaniswa kuzo zonke izikhundla.Intsimbi egciniweyo ineepropati ezinkulu zoomatshini kunye nokuchasa ukubola kwe-intergranular.

Isicelo: Isetyenziselwa i-welding-resistant corrosion 06Cr19Ni10 izakhiwo zensimbi ezingenasici ezinobushushu bokusebenza bungaphantsi kwe-300 ° C.Isenako ukuwelda ezinye iintsimbi ezinokuweldability okulambathayo (ezifana nentsimbi ephezulu yechromium) kunye nemigangatho engaphezulu yentsimbi engatyiwayo.

 

Ukwakhiwa kweekhemikhali zentsimbi edibeneyo(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

9.0 ~ 11.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Iimpawu zobuchwephesha bentsimbi ye-weld:

Into yovavanyo

 

Tensile strength

Mpa

Elongation

%

Iqinisekisiwe

≥550

≥35

 

yangoku eCetyisiweyo:

Intonga yobubanzi

(mm)

2.0

2.5

3.2

4.0

5.0

I-Welding yangoku

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Isaziso:

1. I-electrode kufuneka ibhakwe ngeyure eli-1 kwi-250 ℃ ngaphambi kokusebenza kwe-welding;

2. Ukuxhatshazwa kwe-corrosion kunye nomxholo we-ferrite wensimbi egciniweyo inqunywe yisivumelwano esiphindwe kabini sokubonelela kunye nemfuno.

 

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Siye sabandakanyeka ekwenzenii-electrode ye-weldings, iintonga ze-welding, kwayeukuwelda izinto ezityiwayongaphezu kweminyaka engama-20.

Iimveliso zethu eziphambili ziquka i-electrode yentsimbi ye-welding, i-carbon steel welding electrode, i-alloy welding electrode, i-electrode ye-welding, i-nickel & ne-cobalt alloy welding electrode, intsimbi ethambileyo kunye ne-low alloy welding wires, i-welding steel wire, i-gas-shielded flux cored wire, iingcingo ze-aluminiyam, ukuwelda kwe-arc emanzini.iingcingo, i-nickel & ne-cobalt alloy welding ingcingo, iingcingo zokuwelda zobhedu, i-TIG & ne-MIG iingcingo zokuwelda, ii-electrode ze-tungsten, i-carbon gouging electrode, kunye nezinye izincedisi ze-welding & consumables.


  • Ngaphambili:
  • Okulandelayo: