AWS A5.4 E309-16 Stainless Steel Welding Electrode Welding Consumables Consumables Materials, Welding Stick

Inkcazelo emfutshane:

I-A302 (AWS E309-16) yi-Cr23Ni13 i-electrode yensimbi engenasici kunye ne-titanium-calcium coating.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Stainless Steel Welding Electrode

A302                                      

GB/T E309-16

AWS A5.4 E309-16

Inkcazo: I-A302 yi-Cr23Ni13 i-electrode yensimbi engenasici kunye ne-titanium-calcium coating.Ingasetyenziselwa zombini i-AC kunye ne-DC ngokusebenza okugqwesileyo kokusebenza.Intsimbi ediphozithiweyo inokumelana nokuqhekeka okukhulu kunye nokumelana ne-oxidation.

Isicelo: Isetyenziselwa i-welding uhlobo olufanayo lwensimbi engenasici, i-stainless steel lining, i-special-shaped steel (i-Cr19Ni9 ifana nentsimbi ephantsi ye-carbon), i-chromium ephezulu, i-manganese ephezulu, njl.

 

Ukwakhiwa kweekhemikhali zentsimbi edibeneyo(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

12.0 ~ 14.0

2.0 ~ 4.0

≤0.75

≤0.030

≤0.040

 

Iimpawu zobuchwephesha bentsimbi ye-weld:

Into yovavanyo

Tensile strength

Mpa

Elongation

%

Iqinisekisiwe

≥550

≥25

 

yangoku eCetyisiweyo:

Intonga yobubanzi

(mm)

2.5

3.2

4.0

5.0

I-Welding yangoku

(A)

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Isaziso:

1. I-electrode kufuneka ibhakwe ngeyure eli-1 kwi-150 ℃ ngaphambi kokusebenza kwe-welding;

2. Ngenxa yokuba ubunzulu bokungena bunzulu ngexesha lokuwelda kwe-AC, unikezelo lombane lwe-DC kufuneka lusetyenziswe kangangoko ukufumana ukungena nzulu.kwaye umsinga akufanele ube mkhulu kakhulu ukuphepha ubomvu bentonga ye-welding.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Siye sazixakekisa ekwenzeni ii-electrode zokuwelda, iintonga ze-welding, kunye nezinto ezisetyenziselwa ukuwelda iminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka i-electrode yentsimbi ye-welding, i-carbon steel welding electrode, i-alloy welding electrode, i-electrode ye-welding, i-nickel & ne-cobalt alloy welding electrode, intsimbi ethambileyo kunye ne-low alloy welding wires, i-welding steel wire, i-gas-shielded flux cored wire, iingcingo ze-aluminiyam, ukuwelda kwe-arc emanzini.iingcingo, i-nickel & ne-cobalt alloy welding ingcingo, iingcingo zokuwelda zobhedu, i-TIG & ne-MIG iingcingo zokuwelda, ii-electrode ze-tungsten, i-carbon gouging electrode, kunye nezinye izincedisi ze-welding & consumables.