I-A062 (AWS E309L-16) i-ultra-low carbon Cr23Ni13 i-electrode yensimbi engenasici kunye ne-titanium-calcium coating.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Stainless Steel Welding Electrode

A062                                         

GB/T E309L-16

AWS E309L-16

Inkcazo: I-A062 yi-ultra-low carbon Cr23Ni13 i-electrode yensimbi engenasici kunye ne-titanium-calcium coating.Ingasetyenziselwa zombini i-AC kunye ne-DC.Inomxholo wekhabhoni ephantsi, ngoko ke inokuxhathisa i-intergranular corrosion ebangelwa yi-carbide precipitation ngaphandle kwe-stabilizers ezifana ne-niobium kunye ne-titanium.

Isicelo: Isetyenziselwa uhlobo olufanayo lwesakhiwo sensimbi engenasici, intsimbi edibeneyo, kunye nezixhobo zetsimbi ezikhethekileyo xa kusenziwa i-synthetic fiber, i-petrochemical, kunye nezinye izixhobo.Isenokusetyenziswa kwakhona ukubekwa phezulu kweeleya zenguqu kudonga lwangaphakathi lwemikhumbi yoxinzelelo lwesixhobo senyukliya kunye nokuwelda kwento engaphakathi kwinqaba.

 

Ukwakhiwa kweekhemikhali zentsimbi edibeneyo(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Iimpawu zobuchwephesha bentsimbi ye-weld:

Into yovavanyo

Tensile strength

Mpa

Elongation

%

Iqinisekisiwe

≥520

≥25

 

yangoku eCetyisiweyo:

Intonga yobubanzi

(mm)

2.5

3.2

4.0

5.0

I-Welding yangoku

(A)

50 ~ 70

80 ~ 110

130 ~ 160

160 ~ 200

 

Isaziso:

1. I-electrode kufuneka ibhakwe ngeyure eli-1 malunga ne-150 ℃ ngaphambi kokusebenza kwe-welding;

2. Ngenxa yokuba ubunzulu bokungena bunzulu ngexesha lokuwelda kwe-AC, unikezelo lombane lwe-DC kufuneka lusetyenziswe kangangoko ukufumana ukungena nzulu.kwaye umsinga akufanele ube mkhulu kakhulu ukuphepha ubomvu bentonga ye-welding

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Siye sazixakekisa ekwenzeni ii-electrode zokuwelda, iintonga ze-welding, kunye nezinto ezisetyenziselwa ukuwelda iminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka i-electrode yentsimbi ye-welding, i-carbon steel welding electrode, i-alloy welding electrode, i-electrode ye-welding, i-nickel & ne-cobalt alloy welding electrode, intsimbi ethambileyo kunye ne-low alloy welding wires, i-welding steel wire, i-gas-shielded flux cored wire, iingcingo ze-aluminiyam, ukuwelda kwe-arc emanzini.iingcingo, i-nickel & ne-cobalt alloy welding ingcingo, iingcingo zokuwelda zobhedu, i-TIG & ne-MIG iingcingo zokuwelda, ii-electrode ze-tungsten, i-carbon gouging electrode, kunye nezinye izincedisi ze-welding & consumables.

OEM/ODM:

Siyayixhasa i-OEM/ODM kwaye sinokwenza isivumelwano sokupakisha kuyilo lwakho, nceda uqhagamshelane nathi ngengxoxo yeenkcukacha.