Iintonga zokuWelda ze-AWS E2209-16 zeNtsimbi engaGciniyo, Iintonga zokuFiller ze-Electrode ezigqunywe yiNtsimbi engaGciniyo

Inkcazo emfutshane:

I-AF2209-16 (AWS E2209-16) yi-electrode yentsimbi engenasici ephindwe kabini ene-nitrogen ekhabhoni ephantsi kakhulu ene-titanium-calcium coating.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Ukuwelda kweNsimbi EngagqwaliyoI-electrode

AF2209-16                               

I-GB/T E2209-16

I-AWS A5.4 E2209-16

Inkcazo: I-AF2209-16 yi-electrode yentsimbi engenasici ephindwe kabini ene-nitrogen ekhabhoni ephantsi kakhulu ene-titanium-calcium coating. Ingasetyenziselwa zombini i-AC kunye ne-DC kunye nokusebenza kakuhle. Ngenxa yokuba ine-molybdenum kunye ne-nitrogen, kwaye umxholo wekhabhoni uphantsi kakhulu, isinyithi esigciniweyo sinokuxhathisa kakuhle ukuqhekeka kunye nokugqwala, ngakumbi ukuxhathisa ukugqwala koxinzelelo.

Ukusetyenziswa: Isetyenziswa kakhulu ekudibaniseni uhlobo olufanayo lwezinto zentsimbi engagqwaliyo enekhabhoni ephantsi kakhulu kwimizi-mveliso yepetroleum kunye neye-hydraulic. Njengokudibanisela intsimbi engagqwaliyo ye-022Cr22Ni5Mo3N duplex.

 

Ukwakheka kweekhemikhali zesinyithi esijiyiweyo (%):

C

Mn

Si

Cr

Ni

Mo

N

Cu

S

P

≤0.04

0.5 ~ 2.0

≤0.90

21.5 ~ 23.5

8.5 ~ 10.5

2.5 ~ 3.5

0.08 ~ 0.20

≤0.75

≤0.030

≤0.040

 

Iimpawu zoomatshini zesinyithi esijijekileyo:

Into yovavanyo

Tensile strength

I-Mpa

Ukwandiswa

%

Iqinisekisiwe

≥690

≥20

 

I-current ecetyiswayo:

Ububanzi bentonga

(mm)

2.5

3.2

4.0

5.0

Ukuwelda kwangoku

(A)

50 ~70

80 ~ 110

130 ~ 150

160 ~ 200

 

Isaziso:

1. I-electrode mayibhakwe iyure e-1 malunga nama-250℃ ngaphambi kokuba isebenze nge-welding;

2. Kubalulekile ukucoca umhlwa, isikali seoyile, amanzi, kunye nokungcola kwiindawo zokuwelda ngaphambi kokuba uwelda.

 

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Besibandakanyeka kwimveliso yei-electrode yokuweldas, iintonga zokuweldakunyeizinto ezisetyenziswayo zokuweldakangangeminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka intsimbi engagqwaliyoi-electrode yokuweldaii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engatyiwayo, ii-wire ze-flux cored ezikhuselwe yigesi, ii-wire welding ze-aluminium, i-submerged arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.

 

 


  • Ngaphambili:
  • Okulandelayo: