AWS E7015 iintonga zokuwelda

Inkcazelo emfutshane:

I-AWS A5.1 E7015 i-low-hydrogen sodium coated carbon steel electrode.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-AWS A5.1 E7015 i-low-hydrogen sodium coated carbon steel electrode.

I-E7015 ye-welding electrode kufuneka iqhutywe kwi-DCEP.Inokusebenzisa kakuhle i-welding eyenza ukuba yenze i-welding-position yonke, ine-arc ezinzileyo, ukususa i-slag kulula kwaye ine-spatter ephantsi.Intsimbi egciniweyo inokusebenza kakuhle koomatshini kunye nokumelana nokuqhekeka, okubonelela ngokuqina okuhle kobushushu obuphantsi.

Isicelo

I-AWS A5.1 E7015 isetyenziswa kwi-welding medium-carbon steel kunye nezakhiwo ezine-alloy ephantsi ezifana ne-16Mn, 09Mn2Si, 09Mn2V kunye neentsimbi ezisetyenziselwa ukwakha iinqanawa ezifana ne-A, B, D, E. Ikwasetyenziswa kwiipleyiti zentsimbi kunye izakhiwo zentsimbi zekhabhoni ekunzima ukuzidibanisa.

Ukuhambelana noMgangatho

GB/T 5117 E5015

AWS A5.1 E7015

ISO 2560-BE 49 15 A

Injongo: I-AWS A5.1 E7015 isetyenziswa kwi-welding medium-carbon steel kunye nezakhiwo eziphantsi-alloy ezifana ne-16Mn, 09Mn2Si, 09Mn2V kunye neentsimbi ezisetyenziselwa ukwakha iinqanawa ezifana ne-A, B, D, E. Ikwasetyenziswa kwintsimbi eshinyeneyo. iipleyiti kunye nezakhiwo zentsimbi zekhabhoni ekunzima ukuzidibanisa.

Ukwakheka kwemichiza(%)

Ukuqulunqwa kwemichiza

C

Mn

Si

S

P

Ni

Cr

Mo

V

Ixabiso lesiqinisekiso

≤

0.15

≤

1.60

≤

0.90

≤0.035

≤0.035

≤

0.30

≤

0.20

≤

0.30

≤

0.08

Isiphumo ngokubanzi

0.082

1.10

0.58

0.012

0.021

0.011

0.028

0.007

0.016

Iipropati zoomatshini beMetal eGcithiweyo(iGesi yokuKhusela:CO2)

Into yovavanyo

Rm(MPa)

I-ReL(MPa)

A(%)

I-KV2(J)

-20℃ -30℃

Ixabiso lesiqinisekiso

≥490

≥400

≥20

≥47

≥27

Isiphumo ngokubanzi

550

450

32

150

142

IiMfuno zoVavanyo lweX-Ray kwiBanga loku-I

Isalathiso sangoku(DC+)

Ububanzi (mm)

Φ2.5

Φ3.2

Φ4.0

Φ5.0

I-Amperage(A)

60-100

80-140

110-210

160-230

Amanqaku:

1. I-electrode kufuneka ifudunyezwe kwiqondo lokushisa lama-350 ° C ngeyure eli-1.Preheat intonga nanini na xa isetyenziswa.

2. Ukungcola okufana nomhlwa, amabala e-oyile kunye nokufuma kufuneka kususwe kwindawo yokusebenza.

3. I-arc emfutshane iyadingeka ukwenza i-welding.Indlela ye weld emxinwa iyakhethwa.


  • Ngaphambili:
  • Okulandelayo: