I-AWS ENiFe-CI (Z408) i-Nickel Cast ecocekileyo ye-Iron Welding Electrodes

Inkcazelo emfutshane:

Ilungele ukudityaniswa kwentsimbi ephezulu engwevu kunye nentsimbi ephoswe ngamaqhuqhuva, enjengesilinda, ibhloko yenjini, ibhokisi yegiya, njl.


Iinkcukacha zeMveliso

Iithegi zeMveliso

IZICELO:

Ilungele ukudityaniswa kwentsimbi ephezulu engwevu kunye nentsimbi ephoswe ngamaqhuqhuva, enjengesilinda, ibhloko yenjini, ibhokisi yegiya, njl.

UHLELO:

AWS A5.15 / ASME SFA5.15 ENiFe-CI

JIS Z3252 DFCNiFe

IIMPAWU:

I-AWS ENiFe-CI (Z408) yintsimbi ye-electrode ene-nickel iron alloy core kunye nokunciphisa okunamandla kokugquma kwegraphite.Ingasetyenziswa kwi-AC kunye ne-DC injongo ezimbini, ine-arc ezinzileyo, kwaye kulula ukuyisebenzisa.I-electrode ineempawu zamandla aphezulu, iplastiki enhle, i-coefficient ephantsi yokwandisa umgca kunye nokunye.Ukumelana nokuqhekeka kwentsimbi engwevu kufana naleyo ye-Z308, ngelixa ukuxhatshazwa kwe-crack ye-nodular cast iron kungaphezulu kwe-ENi-CI (Z308).Kwintsimbi etyhidiweyo ene-phosphorus ephezulu (0.2% P), nayo ineziphumo ezilungileyo kwaye ukusebenza kwayo kokusika kungaphantsi kwe-Z308 kunye ne-Z508 kancinane.I-Z408 isetyenziselwa i-welding yentsimbi engwevu kunye ne-nodular cast iron yegumbi

QAPHELA:

Phambi kwe-welding, ii-electrode kufuneka zibhakwe iyure enye ngeqondo lobushushu eliyi-150±10℃ phambi kokusetyenziswa.

Xa ukuwelda, kufanelekile ukuthatha i-weld emxinwa kwaye ubude be-weld nganye akufanele budlule i-50mm.I-Hammer indawo ye-welding ngokukhawuleza ngesando ngokukhawuleza emva kwe-welding ukwenzela ukuphelisa uxinzelelo kunye nokuthintela ukuqhekeka.

Igalelo lobushushu elisezantsi liyacetyiswa.

UYEKELEKO LWEKHEMIKALI YEMETALI ENDIPILEYO(ISIQEQESHO LOBUNZI): %

Izinto

C

Si

Mn

S

Fe

Ni

Cu

Ubunzima bezinye izinto

Ixabiso eliqhelekileyo

0.35-0.55

≤0.75

≤

2.3

≤0.025

3.0-

6.0

60-

70

25-

35

≤

1.0

UKUSHISA IREFRENSI YAMVA:(AC,DC+)

Idayamitha ye-Electrode(mm)

3.2

4.0

5.0

Ubude (mm)

350

350

350

Welding current(A)

90-110

120-150

160-190

Iimpawu zokuSetyenziswa:

I-arc ezinzileyo kakhulu.

Ukususwa okugqwesileyo kwe-slag.

Ukungena akunzulu.

Ubushushu obuhle kunye nokumelana nokubola.

Ukumelana nokuqhekeka okugqwesileyo.