Ii-Electrode ze-Tyue ezisemgangathweni ophezulu ze-AWS A5.11 ENiCu-7 Nickel Based Welding, ii-Nickel Alloy Welding Rods ze-Arc Welding

Inkcazo emfutshane:


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Electrode yokuWelda yeNickel kunye neNickel Alloy

I-Ni207                                                     

GB/T ENi4060

I-AWS A5.11 ENiCu-7

Inkcazo: I-Ni207 yi-electrode ye-Monel alloy ene-hydrogen sodium coating ephantsi. Sebenzisa i-DCEP (i-electrode yangoku ngqo) kwaye isebenza kakuhle ekudibaniseni kunye nokumelana nokuqhekeka.

Ukusetyenziswa: Kwi-welding ye-Monel okanye iintsimbi ezahlukeneyo. Ingasetyenziselwa nomgangatho wotshintsho lwe-welding ye-overlay.

 

Ukwakheka kweekhemikhali zesinyithi esijiyiweyo (%):

C

Mn

Fe

Si

Al

Ti

Cu

Nb

Ni

S

P

≤0.15

≤4.0

≤2.5

≤1.5

≤1.0

≤1.0

27.0 ~ 34.0

≤2.5

≥62.0

≤0.015

≤0.020

 

Iimpawu zoomatshini zesinyithi esijijekileyo:

Into yovavanyo

Tensile strength

I-Mpa

Unikeze Amandla

I-Mpa

Ukwandiswa

%

Iqinisekisiwe

≥480

≥200

≥27

 

I-current ecetyiswayo:

Ububanzi bentonga

(mm)

3.2

4.0

Ukuwelda komsinga

(A)

90 ~ 110

110 ~ 150

 

Isaziso:

1. I-electrode mayibhakwe iiyure ezi-2 malunga nama-300℃ ngaphambi kokuba isebenze nge-welding;

2. Kubalulekile ukucoca umhlwa, ioyile, amanzi, kunye nokungcola kwiindawo zokuwelda ngaphambi kokuba uwelda. Zama ukusebenzisa i-arc emfutshane ukuwelda.

 