I-ELECTRODE YENTSIMBI E-TYUE E308-16 ENGAGQIBELIYO

Inkcazo emfutshane:

I-electrode yokuwelda yohlobo lwe-titanium yomgca wentsimbi engatyiwayo enekhabhoni ephantsi kakhulu.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Udidi:

I-AWS A5.4 / ASME SFA5.4 E308-16

I-JIS Z3221 D308-16

Inkcazo:

I-Electrode yokuWelda yeNtsimbi engaGciniyoI-E308-16 luhlobo lwe-titanium yomgcai-electrode yokuweldakwintsimbi engagqwali enekhabhoni esezantsi kakhulu. Intsimbi ye-weld ineempawu ezintle kakhulu zoomatshini kwaye ibonakalisa ukumelana okuhle nokugqwala phakathi kwe-granular ngenxa yokuba umxholo wekhabhoni okuyo uyi-≤. 0.04% b. Ingasetyenziselwa zonke iindawo zokuwelda kunye nokusebenza okugqwesileyo: i-arc ezinzileyo, amachaphaza amancinci, inkangeleko entle ye-weld. Kwanei-electrode yokuweldaIbonisa ulwazelelelo oluhle lokumelana nobushushu, kulula ukuyijika ibe bomvu kwaye i-gas porosity ayivelisi.

Isicelo:

Ukuwelda kwentsimbi eyi-18%Cr-8%Ni.

Ifanelekile kwizakhiwo zokuwelda ezenziwe ngentsimbi engagqwaliyo ye-022Cr-19Ni10 enekhabhoni ephantsi kakhulu, efana nefayibha yokwenziwa, isichumisi,

izixhobo ze-petrochemical, njl.

Ukwakheka kweekhemikhali zesinyithi esigciniweyo (E308L-16) (%)

Into C Mn Si Cr Ni S P Cu Mo
ixabiso eliqhelekileyo ≤0.08 0.5-2.5 ≤0.90 18.0-21.0 9.0-11.0 ≤0.030 ≤0.040 ≤0.75 ≤0.75
Ixabiso lomzekelo 0.043 1.10 0.78 19.52 9.76 0.012 0.031 0.02 0.032

Iipropati zoomatshini zesinyithi esigciniweyo (%)

Ukusebenza kokulwa nokugqwala kunye nokwakheka kwe-ferrite kufuneka kumiselwe phakathi komthengi nomthengisi.

Into Amandla okuThamba (MPa) Ukwandiswa (%)
ixabiso eliqhelekileyo ≥550 ≥25
Ixabiso lomzekelo 601 41

Ububanzi(mm)

2.0

2.5

3.2

4.0

5.0

Umsinga wokuWelda (A)

25-50

50-80

80-110

110-160

160-200

 

Amanqaku malunga nokusetyenziswa:

1. Gcina i-arc imfutshane kangangoko.

2. Susa ukungcola okufana neoyile nothuli kwi-groove.

3. Yomisa ii-electrodes kwi-350 (662) imizuzu engama-60 ngaphambi kokuba uyisebenzise