Intonga yokuwelda yentsimbi engagqwaliyo ye-E312-16

Inkcazo emfutshane:

I-Electrode yokuWelda yeNtsimbi Engagqwaliyo isetyenziselwa ukuwelda i-29% Cr-9% Ni stainless steels casting, i-xenotransplanation steel kunye ne-harding alloy steel.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Ukuwelda kwe-AWS E312-16 Stainless SteelI-electrodeIntonga

I-Solder/Filler Rod luhlobo lwe-electrode yentsimbi enezigaba ezibini enesigqubuthelo sohlobo lwe-lime-titania. Ngenxa ye-ferrite engama-40% kwisinyithi esigciniweyo, i-solder inokumelana okuhle kakhulu nokuqhekeka. I-Solder inokusebenza okuhle kakhulu kokuqhekeka. I-filler rod isetyenziselwa ukutywina intsimbi enekhabhoni ephezulu, intsimbi yesixhobo, intsimbi enobushushu obuphezulu, intsimbi yezixhobo, intsimbi eyahlukileyo, njl. I-soldering rod inomsebenzi omhle kakhulu wokutywina, ukumelana okuhle nokuqhekeka, kunye ne-electrode yentsimbi enezigaba ezibini enesigqubuthelo sohlobo lwe-lime-titania.

Inombolo yomzekelo: I-electrode yentsimbi engagqwaliyo ye-E312-16

Izinto eziphathekayo: Intsimbi Engagqwaliyo

Ubude: 300mm-500mm

Ububanzi: 2.0mm, 2.5mm, 3.2mm, 4.0mm

Isicelo: Isinyithi somlotha esinamandla aphezulu kunye nokuwelda kwesinyithi sebhola

I-Electrode yentsimbi engenasici enamabakala amabini i-AWS E312-16 GB E312-16
Intshayelelo: I-A1002 luhlobo lwe-electrode yentsimbi enama-phase amabini ene-lime-titania type coating. Ngenxa ye-40% ye-ferrite kwisinyithi esigciniweyo, inokumelana okuhle kakhulu nokuqhekeka. Isebenza kakuhle kakhulu ekudibaniseni.
Ukusetyenziswa: Isetyenziselwa ukuwelda intsimbi enekhabhoni ephezulu, intsimbi yesixhobo, intsimbi enobushushu obuphezulu, intsimbi yezixhobo, intsimbi eyahlukileyo, njl.

Ukwakheka kweekhemikhali zesinyithi esigciniweyo (%)

Ukwenziwa kweeKhemikhali C Mn Si S P Ni Cr
Ixabiso leSiqinisekiso ≤0.15 0.5~2.5 ≤0.90 ≤0.030 ≤0.040 8.0~10.5 28.0~32.0

Iipropati zoomatshini zesinyithi esigciniweyo

Into yoVavanyo I-Rm(MPa) I-A(%)
Ixabiso leSiqinisekiso ≥660 ≥22

Isalathiso sangoku (AC, DC+)

Ububanzi be-Electrode (mm) φ2.5 φ3.2 φ4.0 φ5.0
Umsinga wokuWelda (A) 50~80 80~110 110~160 160~220

Imiyalelo:

1. Ii-electrode mazibhakwe ngaphantsi kwama-250°C kangangeyure ngaphambi kokuba zifakwe kwi-welding.

2. Kungcono ukuba kusetyenziswe umsinga othe ngqo kwaye umsinga akufuneki ube namandla kakhulu.

Ukupakishwa kunye nokuHanjiswa

Iinkcukacha zokuPakisha: 5kgs/ibhokisi, 20kgs/ibhokisi

Iinkcukacha zokuhanjiswa: 20-25days