I-electrode yentsimbi engenasici ye-E316L-16

Inkcazo emfutshane:

Ukuwelda kwe-E316L-16 yekhabhoni ephantsi kakhulu 18%Cr-12%Ni-2%Mo (intsimbi engagqwaliyo engama-316L)


Iinkcukacha zeMveliso

Iithegi zeMveliso

Iintambo zokuWelda ze-AWS A5.4 E316L-16 zentsimbi engagqwaliyo

I-AWS: SFA 5.4 E316L-16

IS: 5206 E19.12.2.LR16

IKHOWUDI YE-ISO YE-EN: 3581-AE 19 12 3 LR 3 2

Iimpawu zokusetyenziswa:

I-E316L-16 yi-electrode yohlobo lwe-lime-titania enikwe ukusebenziseka kakuhle kunye nokudityaniswa.

Njengoko isinyithi esinomatshini wokuwelda yonke sinesakhiwo se-austenite esiqulathe ubungakanani obufanelekileyo be-ferrite, ukumelana nokuqhekeka kulungile. Sinokumelana nokugqwala okuphakathi kwekristale kwimeko edibeneyo kuba umxholo wekhabhoni uncinci kwaye ukumelana nokugqwala okuphakathi kwegranular kungaphezulu kokwe-E316L-16 kwaye sineMo. Ukuxhathisa ubushushu nako kulungile.

I-E316L-16 inokumelana nokufuma okuphezulu kwaye iyakwazi ukumelana neembobo ezintle.

UKWAKHIWA KWEEKHEMIKHALI ZONKE ZESIMBI ESIWELDWE (%)

I-elementi

C

Mn

Si

Cr

Ni

Mo

S

P

Cu

Ipesenti

≤0.04

0.50-2.50

≤0.90

17-22

11-14

2.0-3.0

≤0.030

≤0.04

≤0.75

IIPROPATI ZEZINTO EZINAMATHENI ZE-WELD STEAL

I-UTS

Ukwandiswa

(MPa)

(L= 5d)%

545

40

IDATHA YANGOKU NEYOKUPAKISHA: AC / DC(+)

Ubungakanani (mm)

5×350

4×350

3.15×350

2.5×350

Uluhlu lwangoku (ii-Amps)

150-180

110-140

80-100

60-80

Ubunzima / Ibhokisi (iikhilogram)

2.5

2.5

2.5

2.5

Isilumkiso:

1. Sebenzisa i-arc emfutshane kunye ne-stringer bead ukunciphisa ubushushu.

2. Qinisekisa ukuba ii-electrode zomile. Zomise kwakhona ii-electrode kwi-250-300°C kangangeyure enye.

Amanqaku malunga nokusetyenziswa:

Ububanzi bokuluka bufanele bube ngaphakathi kwezihlandlo ezibini ezinesiqingatha ukusuka kububanzi be-electrode.

Susa ukungcola okufana neoyile kunye nothuli kwi-groove.

Yomisa ii-electrode kwi-350 (662) imizuzu engama-60 ngaphambi kokuba uyisebenzise.


  • Ngaphambili:
  • Okulandelayo: